How can weld lines be prevented behind inserted recasses and letters?

 

Possible cause:

  • Differences in wall thickness

 

Remedies:

  • Reduce injection pressure
  • Increase mold temperature
  • Raise melt temperature
  • Relocate gates
  • Round off sharp-edged transitions
  • Reduce depth of lettering and / or round off edges

 

 